The hybrid hot mirrors consist of metallic and dielectric materials. The transmission peaks at around 75% at 600nm and the IR rejection (>95%) extends out to the FAR infrared. This coating would be used when longwave length rejection is needed and the visible transmission is less important.
Reynard Corporation standard parameters apply:
Substrate Material: Fused Silica
Thickness: 2.3mm ±0.2mm
Surface Quality: 80-50 Scratch & Dig
Parallelism: < 3 Arc Minutes
Environmental: Per MIL-M-13508C
Hardness: Per MIL-M-13508C
Adhesion: Per MIL-M-13508C
Please contact us for current pricing.